This study evaluates the mechanical and biological perfomance of Triply Periodic Minimal Surface (TPMS) scaffolds (gyroid and diamond) in two different lattice topologies (sheet and solid-based) using calcium phosphate-based materials. While natural trabecular bone exhibits a compressive strength of 20–80 MPa, current synthetic scaffolds often struggle to balance structural integrity with bioactivity. We investigated sheet and solid-based TPMS lattice topologies at porosities of 65% and 50%, manufactured using stereolithography of hydroxyapatite (HAp) and beta-tricalcium phosphate (β-TCP) slurries. Mechanical testing showed that solid-based lattice topologies provided superior performance, reaching compression strengths of up to 20 MPa, with solid-based gyroid geometries consistently outperforming diamond structures at porosities above 50%. On the other hand, sheet-based geometries offered compression strength less than 10 MPa across both HAp and TCP. Biologically, while both HAp and β-TCP supported cell proliferation and exhibited similar initial alkaline phosphatase (ALP) activity, HAp demonstrated higher structural strength at the cost of lower long-term bone mineralization. In contrast, β-TCP facilitated higher mineralization, suggesting a faster rate of biological integration. These findings indicate that while solid gyroid HAp scaffolds provide compression strength analogous to trabecular bone, the integration of β-TCP is essential for long-term osteoblast mineralisation. This research provides a framework for optimizing the trade-off between mechanical resilience and biological functionality in the design of next-generation BTE implants.
additive manufacturing; TPMS scaffolds; calcium phosphate ceramics; bone tissue engineering